Sunday, October 08, 2006

After Sanding add a Little Tung Oil



This is how the cabin looks after a first coat of 50% Tung Oil, and 50% thinners... the way this stuff works on fine timbers is simply stunning.

Thanks to Keith Jewell for showing me the way on this, this has to be the best finish for timber.. there is NO varnish on my vessel AT ALL !!


The depth, and warmth of grain will improve further, as more coats of Tung Oil are added.. as I found on my deck.